Polymer Property : Film Tensile Strength at Break, TD = 26.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 26.6 MPa
3860 psi
ASTM D882
ExxonMobil Pax-Plus™ 3204 Blown Film Resin
Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin..