Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 256 MPa | 37100 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 70 MB OPP Film Product Description: Bicor 70 MB is a biaxially oriented polypropylene film for use in metalized film applications. 70 MB, when metalized, is used in adhesive and extrusion laminations to reveres-pr.. |