Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 162.03 MPa
23500 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil OPPalyte® 40 HM OPP Film
White opaque OPP film with a proprietary cavitated core. Designed for cold seal applications and is used as a surface print, monoweb, or as the inside web of a lamination. Information provided by Ex..