Polymer Property : Film Tensile Strength at Break, TD = 23.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 23.9 MPa
3470 psi
ASTM D882
ExxonMobil ESCOR™ AT 320 Blown Film Resin  (discontinued **)
ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 23.9 MPa
3470 psi
ASTM D882
LyondellBasell Plexar® PX3060 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and ..
Film Tensile Strength at Break, TD 23.9 MPa
3470 psi
ASTM D882
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 23.9 MPa
3470 psi
ASTM D882
ExxonMobil LD 306.57 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 23.9 MPa
3470 psi
ASTM D882
ExxonMobil LD 306.75 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical