Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 224.94 MPa | 32625 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 740 Gauge Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and.. |
|||
Film Tensile Strength at Break, TD | 224.94 MPa | 32625 psi | ASTM D882A |