Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 22.24 MPa | 3225 psi | ASTM D882 |
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng.. |