Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 13.8 MPa
2000 psi
ASTM D882
LyondellBasell Petrothene® NA334000 Low Density Polyethylene
ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulat..
Film Tensile Strength at Break, TD 13.8 MPa
2000 psi
ASTM D3759
3M Scotch® 3723 High Performance Cold Temperature Box Sealing Tape
Scotch® Box Sealing Tape 3723 is a high performance packaging tape for application at refrigeration temperatures, or at room temperature with subsequent storage at low temperatures. This product ha..