Polymer Property : Film Tensile Strength at Break, TD = 197 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 197 MPa
28600 psi
Aldrich Single Layer Graphene on PET
PET film base with graphene coating; uniform film and excellent thickness consistency. Its transparency combined with electrical conductivity allows it use in many niche applications.