Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 191 MPa | 27700 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 150LL-302 OPP Film Product Description: A white, corona-treated polypropylene label facestock designed for rigid and semi-rigid pressure-sensitive applications requiring durability, opacity, and excellent graphic appe.. |