Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 12.1 MPa | 1750 psi | ASTM D3759 |
3M Scotch® 610 Cellophane Film Tape Scotch® Cellophane Film Tape 610 is a high performance, transparent cellophane film tape featuring a high tack adhesive system. This product offers excellent adhesion, dispensing and handling prope.. |