Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 175 MPa | 25400 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 52LLC210 Preliminary Data Sheet OPP Film Product Description: A clear gloss, surface-printable polyolefin film with enhanced conformability and squeezability for use in face-stock pressure sensitive applications. The proprietary core const.. |