Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 93.1 - 114 MPa | 13500 - 16500 psi | ASTM D882 |
Honeywell Capran® Unidraw (0.75 mil) Nylon 6 Film
(discontinued **) Description: Capran® Unidraw is a 0.75 mil (19 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str.. |