Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 150 MPa | 21700 psi | 510 |
ExxonMobil Hicor® 30 HT 103 OHD Film One-side treated, non-sealable, oriented high density polyethylene film, which has outstanding stiffness, deadfold, and directional tear characteristics. This film has been designed to be used in va.. |
|||
Film Tensile Strength at Break, TD | 150 MPa | 21700 psi | 510 |
ExxonMobil Hicor® 30 HT 183 OHD Film One-side metallized, non-sealable, oriented high density polyethylene film, which has outstanding deadfold and directional tear characteristics. This film has been designed to be used in various app.. |