Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 15.1 MPa | 2190 psi | ASTM D3759 |
3M Scotch® 313 Box Sealing Tape Scotch® Box Sealing Tape 313 is designed for easy handling and smooth dispensing. The high coating weight of acrylic adhesive makes it ideal for wide temperature swings and applications where it is.. |
|||
Film Tensile Strength at Break, TD | 15.1 MPa | 2190 psi | ASTM D3759 |
3M Scotch® 829 Packing List Pouch Tape Scotch® Packaging List Pouch Tape 829 is a pressure-sensitive tape with a red boarder framing a non-sticky, clear, rectangular center window, which allow attaching and protection of packing lists a.. |