Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 10.3 MPa
1500 psi
ASTM D882
Westlake EF602 Low Density Polyethylene
Westlake EF602 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize..