Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 3919.9 MPa @Pressure 30.0 MPa, Temperature 90.0 °C |
568530 psi @Pressure 4350 psi, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |