Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 2630 MPa @Pressure 10.0 MPa, Temperature 23.0 °C |
382000 psi @Pressure 1450 psi, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Tensile Creep Modulus, 1 hour | 2630 MPa @Pressure 15.0 MPa, Temperature 140 °C |
382000 psi @Pressure 2180 psi, Temperature 284 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |