Mechanical Properties Metric English Comments
Dart Drop Test >= 575 g
>= 1.27 lb
ASTM D1709
M. Holland Company MAGMA® LL1091-AS LLDPE  (discontinued **)
Additives: Medium Antiblock, Medium SlipFeatures: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.