Polymer Property : Dart Drop Test = 57.0 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 57.0 g
0.126 lb
Method A; ASTM D1709
Dow DOWLEX™ 2036G Linear Low Density Polyethylene
Improved thermal stability for high stiffness film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow