Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 490 g | 1.08 lb | ASTM D1709A |
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi.. |