Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 470 g | 1.04 lb | blow ratio: 4:1, frost line: 900mm, thickness:20µm; ASTM D1709-98 |
Ipiranga Petrochem GP 9452 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Dart Drop Test | 470 g | 1.04 lb | ASTM D1709 |
ExxonMobil Exceed™ 1518KC Metallocene Polyethylene Resin Product Description: Exceed 1518KC is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518KC have outstanding tensile, impact strength and puncture. These superior strength propertie.. |