Mechanical Properties Metric English Comments
Dart Drop Test 288 g
0.635 lb
Method A; ASTM D1709
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
DOWLEX™ 2045G resin is designed for the production of a wide variety of industrial and consumer films (though it is not recommended for silage stretch film). The product also delivers very good pr..