Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 232 g | 0.512 lb | Method A; ASTM D1709 |
Dow DOWLEX™ 2056G Linear Low Density Polyethylene Improved thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |