Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 118 g | 0.260 lb | |
Cyclewood Solutions Xylomer™ XM1-GQD Compostable Film Resin 100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an ab.. |