Polymer Property : Dart Drop Test = 1.06 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 480 g
1.06 lb
ISO 7765-1
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa..