Polymer Property : Dart Drop Test = 0.794 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 360 g
0.794 lb
ASTM D1709A
Westlake EMAC® SP2252 20.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2252 is a 20.5% EMA copolymer containing slip and antiblock. This resin is designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal te..
Dart Drop Test 360 g
0.794 lb
ASTM D1709A
ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation. Availability: Africa & M..