Polymer Property : Dart Drop Test = 0.624 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 283 g
0.624 lb
Method A; ASTM D1709
Dow 662I Low Density Polyethylene Resin
Blown Film Resin designed for enhanced bubble stability High melt strength Optimum gauge range: 1.5 - 5.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow