Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 148 g | 0.326 lb | Method B; ASTM D1709 |
Dow DOWLEX™ 2247G Polyethylene Resin Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap.. |