Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop Test = 0.306 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 139 g
0.306 lb
ASTM D1709
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film
Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor..