Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 62.0 g | 0.137 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin, 0.6 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |