Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 49.0 g | 0.108 lb | ASTM D1709 |
Huntsman Rexell® H3108 Cast Film Extrusion LLDPE
(discontinued **) Linear low density octene copolymerApplications: Cast film extrusionFilm properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by Huntsman Corporation |