Polymer Property : Elmendorf Tear Strength, TD = 945 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 37.2 g/micron
945 g/mil
2.5 BUR; ASTM D1922
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film
This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica..