Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 36.91 g/micron | 937.5 g/mil | ASTM D1922 |
ExxonMobil LL 3002.32 Cast Film Resin
(discontinued **) LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, .. |