Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 9.20 g/micron | 234 g/mil | ISO 6383-2 |
Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film Lumicene® mPE M 4040 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 4040 can be processed at high output rates with low extrusion pressure, low neck-in, ex.. |
|||
Elmendorf Tear Strength, TD | 9.20 g/micron | 234 g/mil | ISO 6383-2 |
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra.. |