Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 8.524 g/micron | 216.5 g/mil | ASTM D1922 |
Dow 608A Low Density Polyethylene (LDPE) A formulated clarity film resin for thin gauge optical packaging Optimum gauge range: 0.8 - 2.5 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |