Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 16.0 - 31.0 g/micron | 406 - 787 g/mil | Average value: 20.1 g/micron Grade Count:18 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |