Polymer Property : Elmendorf Tear Strength, TD = 7.80 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 7.80 g/micron
198 g/mil
Dow LDPE 586A Low Density Polyethylene, Packaging Grade
DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio..