Elmendorf Tear Strength, TD 7.60 g/micron
193 g/mil
ASTM-D1922
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene
TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad..