Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.625 g/micron | 66.67 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD 319.92 Film Resin
(discontinued **) Escorene Ultra LD 319.92 is a 9.0 wt% vinyl acetate copolymer film resin, that exhibits superior impact strength and heat sealability.Information provided by ExxonMobil Chemical |