Polymer Property : Elmendorf Tear Strength, TD = 640 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 25.2 g/micron
640 g/mil
ASTM D1922
ExxonMobil EXACT™ 3139 Plastomer for Cast Film Applications
Product Description: Exact 3139 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3139 is designed for both monolayer and multilayer coe..