Polymer Property : Elmendorf Tear Strength, TD = 635 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 25.0 g/micron
635 g/mil
ASTM D1922
Lotte Chemical Titan TITANCEED® mL3564 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL3564 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL3564 have outstanding tensile properties, impact streng..