Elmendorf Tear Strength, TD 6.93 g/micron
176 g/mil
propagated; ASTM D1922
Honeywell Capran® NyLid™ WMB 250 Nylon Lidding Film  (discontinued **)
Description: Capran® NyLid™ WMB 250 is a 2.5 mil, white medium barrier nylon co-extruded film with an EVOH core. Applications: Capran® NyLid™ WMB 250 is suitable for die cutting, readily accepts..
Elmendorf Tear Strength, TD 6.93 g/micron
176 g/mil
ASTM D1922
ExxonMobil EXACT™ 3128 Plastomer for Blown Film Applications
Product Description: Exact 3128 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It is designed fro both monolayer and multilayer coextruded ..