Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 6.40 g/micron | 163 g/mil | ASTM D1922 |
Braskem EB 853/72 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose; automatic packaging of solids products (FFS). Informatio.. |
|||
Elmendorf Tear Strength, TD | 6.40 g/micron | 163 g/mil | ASTM D1922 |