Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 23.2 g/micron | 589 g/mil | |
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance.. |