Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 22.8 g/micron | 579 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 22.8 g/micron | 579 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac.. |
|||
Elmendorf Tear Strength, TD | 22.8 g/micron | 579 g/mil | ASTM-D1922 |
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains antiblock, proc.. |