Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 22.6 g/micron
574 g/mil
ASTM D1922
Chevron Phillips 6109FK Linear low density polyethylene blown film resin  (discontinued **)
Resin Type: linear low density polyethylene, butene copolymer, medium antiblock, medium slip, process aid version of 6109, blown film resinCharacteristics: good stiffness at thin gauges, good drawdo..