Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 21.399 g/micron
543.53 g/mil
ISO 6383-2
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH..