Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.100 g/micron | 53.33 g/mil | ASTM D1922 |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Elmendorf Tear Strength, TD | 2.100 g/micron | 53.33 g/mil | ASTM D1922 |
ExxonMobil LD 306.75 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |