Polymer Property : Elmendorf Tear Strength, TD = 507 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 20.0 g/micron
507 g/mil
ASTM D1922
Dow ELITE™ 5400G Enhanced Polyethylene Resin
™ 5400G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking tendencies for good performanc..