Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 19.8 g/micron
503 g/mil
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade
DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g..